News, technical articles and suppliers for the coil winding industry

Coiltech Germany 2027, 17-18 March 2027, Messe Augsburg - international coil and winding exhibitionAdvertisement
Article

Continuous Annealing of Copper Wire: Purpose and Process

By Fang Deng | 15 Nov 2026

Copper that has been drawn is hard and stiff. Annealing softens it so it can be wound into a coil. Continuous annealing does this while the wire runs through, instead of in a furnace holding a whole coil.

Why drawn copper must be annealed

As wire is pulled through dies, it becomes work-hardened. A wire maker explains that this increases tensile strength but severely reduces ductility and flexibility. Annealing heats the wire to its recrystallisation temperature and cools it under controlled conditions. It relieves internal stress, lowers tensile strength and increases elongation. A university teaching module explains the cause in terms of dislocations: deformation introduces them, and annealing forms new strain-free grains that remove them.

What happens as the temperature rises

A study of fine copper bonding wire gives one example of the stages. In that wire, recovery occurred at 300 to 350 C, with strength and hardness decreasing and elongation rising, and recrystallisation at 350 to 460 C, where elongation rose quickly. It was a specific fine wire with trace additions, so the temperatures are an illustration, not a rule for magnet wire. Another source gives a general recrystallisation range of 400 to 700 C depending on alloy and temper.

The continuous method

Wire runs through the annealer at line speed. Historic technical papers from the wire industry describe continuous resistance annealing, in which the wire is heated by electric current as it passes through, and its use together with wire drawing. Annealing can also be done in an oven in the enamelling line. A manufacturer describes an annealing oven as the first step of the enamelling process, where the bare wire is annealed for the necessary softness of the copper.

Effect on conductivity

Soft annealed copper is the baseline for the 100 percent IACS conductivity standard. One article explains that cold drawn copper has slightly lower conductivity because defects scatter electrons, and that annealing restores it to near 100 percent IACS. See the discussion of copper properties in your wire's datasheet.

Annealing and the in-line comparison

One magnet wire maker compared wire made by the conventional method, with drawing and enamelling separated, against its in-line method. For 0.4 mm wire it reports elongation of 30 percent and breaking strength of 254 N/mm2 for the conventional wire, and 40 percent and 274 N/mm2 for the in-line wire. It explains that the smaller area reduction between anneals in the in-line process reduces the driving force for annealing and raises the annealing temperature needed. These are one maker's own results, so use them to understand the trend and not as targets.

What to check

  1. Elongation at break, from the maker's tests.
  2. Tensile strength, which falls when the wire is fully annealed.
  3. Surface: wire must leave the annealer free of oxidation. A manufacturer notes that drawing immediately before enamelling avoids oxidation.
  4. Springback and winding behaviour in your own process.

Frequently asked questions

What is continuous annealing?

Softening the wire by heating it as it runs, not in a batch.

What does annealing change?

It lowers tensile strength and increases elongation, and restores conductivity close to 100 percent IACS.

How is the wire heated?

By resistance heating or in an oven, among other methods.

What temperature is used?

It depends on the wire and process. A general range for recrystallisation is 400 to 700 C. Use the maker's data.

Does annealing affect resistance?

It restores conductivity lost to cold work.

Sources

  • New England Wire Technologies: what is annealing in wire manufacturing (work hardening, softening, IACS baseline)
  • Materials Education: work hardening and annealing of copper (dislocations, recrystallization)
  • FCT Metal: understanding the annealing process and copper wire flexibility (recrystallization, conductivity recovery)
  • Materials Research Innovations 2015: copper bonding wire during continuous annealing (recovery and recrystallisation temperature ranges for a specific fine wire)
  • Wire Association International: abstract of Continuous resistance annealing of copper wire (Furukawa Electric, 1970)
  • Elektrisola: fine and ultrafine enamelled wire production flow (8 mm rod, annealing oven, enamel applicator, curing oven)
  • CMP Controls: copper and aluminium magnet wire guide (8 mm rod, in-line drawing, annealing and enamelling)