Common Defects in Fine Copper Wire Drawing

By Vladimir Frolov | 18 Nov 2026

Fine magnet wire is thin and has to be drawn many times, so small faults matter. A metallurgist from a wire maker writes that, with respect to defects, fine magnet wire and shaped wire are the most critical products to produce.

Defects that start in the rod

The same source says copper rod defects often originate in the continuous casting and rolling process. They include slag and copper oxide inclusions, hot cracks, slivers, fold-over of the cast bar corners, insufficient removal of scale and coining of oxide particles into the rod surface. Most of the intermetallic inclusions are brittle and act as sites where cracks start and spread in the drawn wire. A teaching presentation on drawing lists seams, slivers and pipe as defects in the starting rod.

Oxide film

Copper wire always carries a residual oxide film from the hot rod stage. The metallurgist says it is standard practice to measure film thickness by a coulometric reduction test. The films can be harmful: they may lead to defects during drawing, excessive wear of the drawing dies, inadequate solderability and poor adhesion of the enamel to the conductor. See cleaning copper wire before insulation application.

Defects from drawing itself

The same article says the largest single class of surface defects comes from wire drawing, and shows as die marks, mechanical damage, gouges or slivers on the bare conductor. Surface damage is frequently caused by misalignment of the moving wire within the machine, or by the compaction of copper fines inside the throat of the die. A teaching presentation lists further defects in cold drawn products:

  • Longitudinal scratches, from a scored die, poor lubrication or abrasive particles.
  • Slivers, from swarf drawn into the surface.
  • Internal cracks, from pre-existing defects in the rod or from overdrawing.
  • Centre burst, or chevron cracking, which occurs for low die angles at low reductions.

An equipment maker adds that scratches usually appear as longitudinal marks, and lists worn dies, contaminated lubricant, improper die installation and foreign particles as typical causes. It lists wire breakage causes as too much reduction per pass, incorrect drawing speed, material defects and unstable tension.

How makers control them

  • Regular die inspection and replacement.
  • Clean, well managed lubrication.
  • Stable wire guiding and tension.
  • Rod quality checks.
  • Eddy current testing on the line. See the article on surface quality for how that works.

Why it matters downstream

A surface flaw on the conductor can show up later in enamel adhesion and insulation reliability, as one equipment maker notes for magnet wire. See pinholes in magnet wire insulation for a related failure in the insulation.

Frequently asked questions

Where do most surface defects come from?

A metallurgist at a wire maker says the largest single class comes from wire drawing.

What causes die marks and scratches?

Worn or scored dies, contaminated lubricant, misalignment and foreign particles.

What is a sliver?

A thin flake of metal pressed into or drawn from the surface. Sources attribute them to swarf, rod defects or drawing problems.

Can rod defects reach the final wire?

Yes. Inclusions and slivers in the rod can start cracks in drawn wire.

How are defects found?

Often by eddy current testing in the line, plus visual and microscopic checks.

Sources

  • Copper Development Association, Innovations 1997: The Metallurgy of Copper Wire (Essex Group metals laboratory; surface oxide, rod defects, drawing defects, annealing, 90 percent reduction practice)
  • Wire drawing presentation: defects in rod and wire drawing (scratches, slivers, fissures, internal cracks, centre burst)
  • CRM drawing machines: common defects in copper wire drawing (supplier; scratches, breakage, causes and prevention)
  • Magnetic Analysis Corp.: how to use eddy current technology to test wire (seams, cracks, pits, slivers; encircling coil and rotary probe)