Copper Wire Surface Quality: Inspection and Acceptance
Surface defects on the copper conductor can lead to problems later with the enamel, as noted in the article on drawing defects. Makers inspect for them during production. Here is how, and where acceptance limits come from.
Eddy current testing
A supplier of test equipment describes eddy current testing as a technique for detecting surface seams, cracks, pits, slivers and internal discontinuities in wire. In an encircling coil test, the wire passes through a coil excited by alternating current. In a rotary probe test, probes traverse the surface. The supplier says encircling coil testing can cover the whole range of wire sizes it lists, from below 0.051 mm up to 18.42 mm, while rotary probe inspection is for larger sizes above 5.08 mm.
A production example
The same company describes an installation at a rod and wire producer where the test sits after annealing and before tensioning and coiling, on a line running up to 22 metres per second. It detects typical small surface defects such as scratches, cracks and pinholes. Vibration at high speed can interfere, so the wire is guided and held. Grading software scores each segment or coil, the customer specifies the number and type of defects per grade, up to 24 defect categories are counted separately, and reports go out with a coil ID. This is one supplier's description of one installation.
The standard
EN 17263:2019 specifies a fully automatic eddy current procedure with an encircling coil for detecting defects on the surface of copper and copper alloy rods, bars, hollow rods and wires. Its scope says the size range and the acceptance level are defined in the relevant product standards. So the test method is general. The pass or fail level comes from the product standard or from agreement with the buyer.
Other checks
- Visual inspection and microscopy of samples.
- Coulometric measurement of oxide film on the copper surface, which a wire-maker metallurgist describes as standard practice.
- Dimension checks. See the article on measuring diameter and ovality.
- Insulation tests after enamelling. See pinholes in magnet wire insulation.
What a buyer can ask for
- Which surface test the maker uses, and where in the line.
- The acceptance criteria and the standard they come from.
- How coils are graded and what is done with coils that fail.
- Any agreed limits on defect type or number for your order.
Do not invent a limit. If the product standard or the supplier does not give one, agree it in writing.
Frequently asked questions
What does eddy current testing find?
Surface seams, cracks, pits, slivers and some internal discontinuities, according to one test equipment maker.
Who sets the acceptance level?
The product standard, or the buyer and supplier by agreement. EN 17263 leaves it to the product standards.
Is the test done on finished wire?
One example tests bare wire after annealing, before coiling.
Can it find every defect?
No test finds everything. Combine methods.
Does a pass mean the enamel will be perfect?
No. It is one check on the conductor, not on the insulation.
Sources
- Magnetic Analysis Corp.: testing small diameter copper rod and wire during drawing (eddy current test after annealing; scratches, cracks, pinholes)
- Magnetic Analysis Corp.: how to use eddy current technology to test wire (seams, cracks, pits, slivers; encircling coil and rotary probe)
- SIS: EN 17263:2019 eddy current testing of copper rods, bars and wires by encircling coil (scope; acceptance levels set in product standards)
- Copper Development Association, Innovations 1997: The Metallurgy of Copper Wire (Essex Group metals laboratory; surface oxide, rod defects, drawing defects, annealing, 90 percent reduction practice)
- Eddywise: copper wire inspection (eddy current systems for surface defects and impurities; supplier)