News, technical articles and suppliers for the coil winding industry

Coiltech Germany 2027, 17-18 March 2027, Messe Augsburg - international coil and winding exhibitionAdvertisement
Article

Solderability and Thermal Bonding in Magnet Wire

By Will Hibbard | 14 Nov 2026

Two features save steps in coil production. A solderable enamel lets you make a joint without first removing the insulation. A bondcoat lets the winding be held together by heat instead of a bobbin or varnish. Each comes with limits.

Solderable enamels

A distributor's guide lists polyurethane as a tough, flexible coating with good dielectric strength that solders at low temperatures without prior removal of the enamel. It also notes that polyurethane is not compatible with all impregnating varnishes and has a limited shelf life. The same guide lists solderable polyesterimide, which adds the thermal and solvent resistance of polyesterimide, solderability without stripping, and compatibility with impregnating varnishes.

One manufacturer datasheet for a solderable polyurethane wire with a bondcoat states a thermal index of 160 C and solderability at 390 C without previous removal of the enamel. Treat that as a figure for that product. Other products have other figures.

How a bondcoat works

A bonding wire has an outer layer on top of the enamel. When heat is applied, the layer softens and sticks the turns together. The datasheet above describes windings made without supporting bobbins and without impregnation, by moulding or pressure, with a bonded coil comparable to trickle-resin or impregnated coils. For types and uses, see self-bonding magnet wire.

The same datasheet gives its conditions. The bonding temperature is between 170 and 200 C depending on the bondcoat, and the energy applied must be accurate. Bonding can be done by Joule heating, passing current through the coil, and it gives a formula for a coil's mass, resistance, current and time. Use the formula and values your wire maker supplies for your wire, not a number from another product.

Choosing between them

  • Terminations that must be soldered directly: look for a solderable enamel. Check the soldering temperature and time the maker states.
  • Coils without a bobbin or varnish: look for a bondcoat. Check the bonding temperature and method.
  • Both: some products combine the two, with a compromise between solderability and bonding noted by the maker.
  • Thermal rating: compare the thermal index with your application. See thermal class of magnet wire.
  • Varnish compatibility: confirm it, especially with polyurethane.

Practical checks

  1. Read the datasheet for the soldering and bonding conditions.
  2. Make trial joints and trial bonded coils with your own equipment.
  3. Inspect each trial joint against your acceptance criteria and the maker's guidance.
  4. Test the coil after bonding, including insulation checks.
  5. Store the wire as the maker advises, since polyurethane has a limited shelf life.

If your wire cannot be soldered through its enamel, strip it first. See how to strip enamelled copper wire safely.

Frequently asked questions

Can all enamelled wire be soldered without stripping?

No. Solderable types such as polyurethane and solderable polyesterimide can. Others need the enamel removed first.

What temperature is used to solder polyurethane wire?

It depends on the product. One datasheet states 390 C without removing the enamel. Use your maker's figure.

What does a bondcoat do?

It is an outer layer that softens with heat and sticks the turns together.

How is a bonded coil heated?

By oven or by passing current through the coil. One maker gives a bonding temperature between 170 and 200 C, depending on the bondcoat.

Does polyurethane wire last forever on the shelf?

No. A distributor guide notes a limited shelf life.

Sources

  • Essex Solutions: Magnebond UL-180 datasheet (solderable polyurethane with polyamide bondcoat; 390 C solderability, 170 to 200 C bonding, Joule heating)
  • CMP Controls: copper and aluminium magnet wire guide (polyurethane and solderable polyesterimide enamels)