Enamel goes on the wire as a liquid. It becomes insulation only after it is cured in an oven. How well that happens has a direct effect on how the finished wire performs.

What happens in the oven

A university thesis on enamelling describes the curing step as a sequence: evaporation of solvents, an increase in the molecular weight of the polymer chains, cross-link reactions where the polymer has reactive groups or cross-linking agents, and intra-chain reactions such as ring closure. The end result is an insoluble, infusible film on the wire surface. The thesis puts the oven temperature at 500 to 700 C, with six to eight coats applied one after another. The application side is covered in how enamel coating is applied to copper wire.

Why thin coats help

The same thesis says thin films can be cured quickly, which lets line speed rise, and that multiple coats cover tiny blow-holes caused by rapid solvent vaporisation. See pinholes in magnet wire insulation for what happens when they are not covered.

Degree of cure changes the properties

A technical bulletin from a polyimide enamel supplier says that many properties of coated wire depend on the degree of cure, and that wire makers and users should select the degree of cure that gives the balance of properties they need. It gives one example: for its enamel in contact with water at elevated temperature in a sealed system, thoroughly cured wire performs best. That is one product. Other enamels behave differently, so ask the maker.

How cure is controlled

  • Process settings: oven temperature, line speed and the number of coats are matched to the wire size and the enamel.
  • Test control: the same bulletin recommends the dissipation factor test for controlling degree of cure in production and says NEMA MW 1000 lists a limit of no greater than 0.006 for wire coated with that enamel. Note that this limit is for that enamel, as stated in the bulletin, and MW 1000 is now MW 01000. Other control tests it names are weight loss at elevated temperature and crazing tendency.
  • Standard tests on the finished wire, such as continuity and breakdown voltage. See breakdown voltage test for enamelled copper wire.

What to ask a supplier

  1. Which test the maker uses to control cure.
  2. Whether a change of enamel batch or oven setting changes the lot's properties.
  3. Data on flexibility, adhesion and thermal endurance for your lot. See thermal class of magnet wire.
  4. Storage and shelf life advice, since some enamels age.

Frequently asked questions

What is curing?

Baking the enamel so the solvent leaves and the resin chains grow and cross-link into a solid film.

What temperature are curing ovens?

One thesis gives 500 to 700 C for the oven. Wire temperature differs. Ask your maker.

Can undercured wire be a problem?

The properties depend on the degree of cure, so yes, a wire can differ from its datasheet.

How is cure checked?

One supplier recommends the dissipation factor test, plus weight loss and crazing tests.

Is each enamel cured the same way?

No. Each has its own schedule.

Sources

  • Ezio Leone, University of Camerino PhD thesis 2022: performance electrical insulation resins (curing step: solvent evaporation, molecular weight increase, cross-linking)
  • Industrial Summit Technology: Pyre-M.L. wire enamel technical bulletin (supplier; dependence of properties on degree of cure, dissipation factor, water and dielectric liquids)
  • YIDA Wire Industry: how enamelled wire is made (supplier; coats per wire, curing and testing)